Mixing
Density and slump
The checks are made with a one litre cylinder at the start of each shift, after any marked change in temperature, and whenever the mix looks wrong. Use the second mix of the shift, because the first can be affected by cleaning water left in the machine. It helps if the same person does the test each time.
Thickness
- Measure with a fireproofing thickness gauge at least every 3 metres on each coated face of the flanges and web.
- Record every reading and work out the average.
- The specified thickness is a minimum. The recommended tolerance on the average is 0 to +3 mm unless the contract says otherwise.
- No single coat, of Fendolite-MII or Fendolite-TG, should be less than 8 mm thick.
We supply fire protection depth gauges for this check.
Estimating quantities
As a guide, Promat give a theoretical yield of 62 m² per tonne at 25 mm thick with minimal wastage. Real coverage varies with the applied density, the accuracy of the thickness, solid filling of small sections, the finish and wastage, so allow for that when ordering.
Checking older stock
Bags stored off the ground and under cover keep for the shelf life on the product data sheet. Stock that is older, or has been stored badly, can be checked before use: look for lumps, make a trial mix, check the density and slump, and spray a sample to confirm it adheres.